WEKO3
アイテム
Spatio-temporal charge behavior in electric double layer capacitors observed by pulsed electro acoustic method
http://hdl.handle.net/10458/2890
http://hdl.handle.net/10458/2890d08d768e-1aa2-4445-95c3-2e32ac0b592c
名前 / ファイル | ライセンス | アクション |
---|---|---|
![]() |
|
Item type | 学術雑誌論文 / Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2010-05-31 | |||||
タイトル | ||||||
タイトル | Spatio-temporal charge behavior in electric double layer capacitors observed by pulsed electro acoustic method | |||||
言語 | en | |||||
言語 | ||||||
言語 | eng | |||||
キーワード | ||||||
言語 | en | |||||
主題Scheme | Other | |||||
キーワード | Electric double layer capacitors, Pulsed electro acoustic method, nanoporous carbon, Charge behavior | |||||
資源タイプ | ||||||
資源タイプ | journal article | |||||
著者 |
Tashima, Daisuke
× Tashima, Daisuke× Kurosawatsu, Kenji× 成, 烈汶× Otsubo, Masahisa× Honda, Chikahisa |
|||||
内容記述 | ||||||
内容記述タイプ | Other | |||||
内容記述 | The use of the pulsed electro acoustic (PEA) method allowed us to perform the direct observations of spatio-temporal charge distributions in EDLCs based on polarizable nanoporous carbonaceous electrode. The negative charge density became the maximum, about -198 C/m3 at the region where was near to anode layer in EDLCs for case of dc voltage 2.5 V, while the positively charged density became the maximum, about 60.1 C/m3 at the region where it was located around the cathode layer. The behavior of negative and positive charges measured by the PEA method reflected the hetero-charges distribution in EDLCs. The performance of the sample was found to be better in terms of the capacitance (Cs) with a maximum value of 55.4 F/g. | |||||
言語 | en | |||||
書誌情報 |
en : Electrochimica acta en : Electrochim. acta 巻 52, 号 15, p. 5071-5075, 発行日 2007-04-20 |
|||||
出版者 | ||||||
出版者 | Pergamon Press | |||||
言語 | en | |||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 00134686 | |||||
書誌レコードID | ||||||
収録物識別子タイプ | NCID | |||||
収録物識別子 | AA00633261 | |||||
著者版フラグ | ||||||
出版タイプ | AM |